• Steel Media Burnishing Guide: How It Creates Mirror Shine and When Not to Use It
    Steel Media Burnishing Guide: How It Creates Mirror Shine and When Not to Use It Aug 27 , 2026
    Steel Media Burnishing Guide: How It Creates Mirror Shine and When Not to Use It Steel finishing media • Pins, balls & discs • Burnishing process, compound pairing and limits Steel media is unique in mass finishing: it is the only media that polishes almost entirely without cutting. Hardened stainless pins, balls, and discs rub against parts under compound pressure, compressing micro-peaks int...
  • Walnut Shell vs Corncob: How to Choose Dry Tumbling Media for Eyewear, Jewelry & Hardware
    Walnut Shell vs Corncob: How to Choose Dry Tumbling Media for Eyewear, Jewelry & Hardware Aug 26 , 2026
    Walnut Shell vs Corncob: How to Choose Dry Tumbling Media for Eyewear, Jewelry & Hardware Dry finishing media selection guide • Walnut shell & corncob • For dry tumbling, vibratory and centrifugal lines Dry organic media — crushed walnut shell and ground corncob — is the workhorse of dry tumbling and dry vibratory finishing. The two materials look similar in the bag, but they behave very d...
  • Mass Finishing for 3D Printed Parts: Deburring and Polishing Additive Manufacturing Components
    Mass Finishing for 3D Printed Parts: Deburring and Polishing Additive Manufacturing Components Aug 26 , 2026
    Mass Finishing for 3D Printed Parts: Deburring and Polishing Additive Manufacturing Components Additive manufacturing post-processing • Deburring, smoothing & polishing • FDM, SLA/DLP, SLS & metal AM parts 3D printing turns out parts close to final shape, but almost never close to final surface. Support scars, layer lines, partially fused powder, and sharp edges stand between a fresh print...
  • Double-Deck Bamboo Tumbling Machine: Standard Operating Procedure, Control Guide & Finishing Recipes
    Double-Deck Bamboo Tumbling Machine: Standard Operating Procedure, Control Guide & Finishing Recipes Aug 19 , 2026
    Double-Deck Bamboo Tumbling Machine: Standard Operating Procedure, Control Guide & Finishing Recipes Model Series: SP-TB4 / SP-TB8 • Precision Dry Tumbling System • Official operation manual The SP-TB Series double-deck bamboo tumbling machine is a precision dry tumbling system designed for high-gloss finishing of premium eyewear frames (acetate, propionate), fine hardware, jewelry, and luxury...
  • Mass Finishing Sample Trial Record for Small Precision Parts
    Mass Finishing Sample Trial Record for Small Precision Parts Jul 20 , 2026
    Printable Process-Control Resource Mass Finishing Sample Trial Record for Small Precision Parts Use this non-promotional worksheet to define the incoming part, record one controlled finishing trial, compare results, and decide whether the process is ready for a repeat run. Important: This record does not replace a drawing, control plan, safety procedure, material compatibility review, or customer ...
  • How to Deburr Small Fasteners Without Damaging Threads, Points, or Recesses
    How to Deburr Small Fasteners Without Damaging Threads, Points, or Recesses Jul 17 , 2026
    Small Parts Finishing Guide How to Deburr Small Fasteners Without Damaging Threads, Points, or Recesses Screws, bolts, nails, pins, and rivets can be processed in bulk, but their functional features make them less forgiving than simple metal blanks. The right mass finishing process must remove loose burrs while protecting threads, points, drive recesses, hollow sections, and dimensional fit. Small...
  • How to Prevent Water Spots, White Film, and Cloudy Stainless Steel After Tumbling
    How to Prevent Water Spots, White Film, and Cloudy Stainless Steel After Tumbling May 28 , 2026
    Wet Finishing Troubleshooting How to Prevent Water Spots,White Film,and Cloudy Stainless Steel After Tumbling A stainless steel part can look clean while wet and develop spots,h
  • How to Separate Small Parts from Tumbling Media: Screens, Size Control, and Process Design
    How to Separate Small Parts from Tumbling Media: Screens, Size Control, and Process Design May 26 , 2026
    Production Separation Guide How to Separate Small Parts from Tumbling Media: Screens, Size Control, and Process Design A finishing cycle is not production-ready until parts can be separated from media repeatedly. This guide explains how part geometry, media wear, screen design, orientation, and external separation methods affect labor, carryover, and the risk of trapped media. Part-media separatio...
  • How to Achieve Mirror Finish on Stainless Steel with Mechanical Polishing
    How to Achieve Mirror Finish on Stainless Steel with Mechanical Polishing May 25 , 2026
    Surface Finishing How to Achieve Mirror Finish on Stainless Steel with Mechanical Polishing This guide covers the key factors to consider when planning a surface finishing process

#+86-592-2381506

Email : info@surface-polish.com

Headquarters address : No. 31, Xinchang Road, Xinyang Industrial Zone, Haicang District, Xiamen

click here to leave a message

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.

Preparing secure enquiry form…